Cutting Tools for Titanium and Heat-Resistant Alloys

Heat-resistant alloys hold their strength at the temperature a cut generates, so the heat stays in the tool instead of leaving with the chip. Precimill supplies sharp AlTiN and AlCrN coated tooling, through-coolant drills, and variable-pitch end mills for titanium and nickel alloys.

These materials are specified for their ability to keep their strength when hot, which is exactly the property that makes them difficult to machine. In ordinary steel the chip carries most of the heat away; in titanium and nickel alloys it does not, so the cutting edge absorbs it until it softens and deforms.

Why the heat stays in the tool

Cutting generates heat by deformation and friction. In steel, a large proportion leaves with the chip because the chip is hot and the material conducts heat reasonably. In titanium the thermal conductivity is low, so the heat has nowhere to go except into the tool.

In nickel alloys the mechanism is different but the outcome is similar: the material retains strength at high temperature, so the deformation zone stays narrow and the heat concentrates at the edge rather than spreading into the chip.

Heat-resistant alloys and tooling response
AlloyFailure modeTooling response
Titanium grade 5Edge softening, galling, spring-backSharp AlTiN edge, low speed, high coolant flow
Commercially pure titaniumGalling and smearingVery sharp polished edge, generous lubrication
Inconel 718Notch wear, extreme heatAlCrN, strong edge preparation, through-coolant
Waspaloy and similarNotch wear, work hardeningAlCrN, varied depth of cut, conservative speed
Cobalt-chromeAbrasion plus heatAlCrN or AlTiN, robust edge, reduced speed

Cutting speed is the lever, not feed

With these alloys the cutting speed has to fall, often substantially, because edge temperature rises with speed. Feed per tooth can usually be maintained or even increased, because a heavier chip carries more heat away per unit of edge contact.

That combination, lower speed and adequate feed, is the opposite of the instinct to slow everything down. Running slowly at a light feed rubs the material and work-hardens it, which is worse than either parameter alone.

Notch wear at the depth-of-cut line

In nickel alloys the tool wears fastest where it enters and leaves the cut, producing a notch that grows until the edge breaks. Varying the axial or radial depth between passes so the notch does not form at the same place is the most effective single countermeasure.

A stronger edge preparation and a coating with high oxidation resistance such as AlCrN also help, but neither substitutes for varying the depth of cut.

Coolant delivery at depth

Through-tool coolant is frequently essential rather than optional, because these operations are often deep pockets or deep holes where flood coolant never reaches the cutting zone.

High pressure is what makes through-tool delivery work: the coolant has to reach the edge with enough velocity to break the vapour barrier that forms at the high temperatures involved. A low-pressure supply through the tool is largely wasted.

Frequently asked questions

Why do titanium tools fail so quickly?

Because titanium conducts heat poorly, so the heat generated by cutting stays in the tool rather than leaving with the chip, and the edge softens and deforms. It also work-hardens and springs back. The response is lower speed, adequate feed and high-flow coolant.

Should I reduce the feed when machining Inconel?

Reduce the speed, but keep the feed adequate. A heavier chip carries heat away per unit of edge contact, so a light feed rubs the material and work-hardens it, which is worse than running at a proper feed per tooth.

How do I stop notch wear on nickel alloys?

Vary the depth of cut between passes so the notch does not form at the same point on the edge. Combine that with a strong edge preparation and an AlCrN coating, but the depth variation is the most effective single measure.

Is through-coolant tooling necessary for these alloys?

Frequently yes. These operations are often deep pockets or holes where flood coolant cannot reach the cutting zone, so through-tool delivery at high pressure is the only way to get coolant to the edge and break the vapour barrier.

Which coating for titanium and nickel alloys?

AlTiN for titanium, where a sharp edge and hot hardness matter, and AlCrN for nickel alloys, where oxidation resistance at very high temperature is the requirement. In both cases the edge preparation is as important as the coating.

Tell us the operation, get a tool recommendation

Send the operation, the workpiece material and its hardness, the machine interface and the diameter and depth you need. We reply within 8 working hours with a geometry, substrate and coating recommendation, and for specials a drawing for approval before anything is ground.

Tool drawings and part numbers can be emailed to [email protected]. We reply within 8 working hours. We do not share customer drawings or tooling with other customers.